Problem: AI Cold Plate Flatness Fails After Finish — Keep the Thermal Face Clean

Problem: accelerator cold plates meet thickness in-process, then after anodize or plating the contact face bows past 0.05–0.1 mm and TIM / liquid interface leaks heat.

Root cause: whole-part cosmetic finish with no masking; copper chosen late without lead-time buffer; sealing ports underspecified on the PDF.

Fix: as-machined thermal face; mask threads / ports; lock Al vs Cu on the first quote; sample flatness before ship.

Lead sketch: Standard ≈ 8–10 days with finish; Express when blank + light finish allow. Courier days stay separate.

Next: open the AI hardware industry page, then upload STEP + PDF on the quote page with flatness callouts.

AIQuoteEmail
PDF

Email kerja sing disenengi ([email protected]). Mail pribadi ora apa-apa. Opsional — download isih bisa.

Kita bakal nggunakake email karya iki mung kanggo ngirim item iki lan kanggo njawab pitakonan engineering (quote, wektu timbal, gambar).

Problem: AI Cold Plate Flatness Fails After Finish — Keep the Thermal Face Clean — Zoryra Precision