Adaty Standart ~10 gün (önüm + howa çyzgy) · Express ~6 gün · çyzgy / DFM

2026-08-10 · 4 min

Problem: AI Cold Plate Flatness Fails After Finish — Keep the Thermal Face Clean

Problem: accelerator cold plates meet thickness in-process, then after anodize or plating the contact face bows past 0.05–0.1 mm and TIM / liquid interface leaks heat.

Root cause: whole-part cosmetic finish with no masking; copper chosen late without lead-time buffer; sealing ports underspecified on the PDF.

Fix: as-machined thermal face; mask threads / ports; lock Al vs Cu on the first quote; sample flatness before ship.

Lead sketch: Standard ≈ 8–10 days with finish; Express when blank + light finish allow. Courier days stay separate.

Next: open the AI hardware industry page, then upload STEP + PDF on the quote page with flatness callouts.

AITeklibiEmail
PDF

Iş e-poçtasy peýdalanylýar (ad@kompaniýa.com). Şahsy poçta hem mümkin. Islegine görä — ýüklemegiň işi hâli-de işleýär.

Bu iş e-poçtasyny diňe şu elementi ibermek we in engineering soraglaryňyza (bahalandyrma, taýýarlama wagty, çyzgylar) jogap bermek üçin ulanar.

Problem: AI Cold Plate Flatness Fails After Finish — Keep the Thermal Face Clean — Zoryra Precision