Material match
Passivation is intended for stainless families. Aluminum should use anodize instead.
Zoryra Precision
Restore corrosion resistance after machining stainless — typical for SS304 / SS316 export jobs.
Passivation is intended for stainless families. Aluminum should use anodize instead.
SS304 / SS316 export jobs often add passivation after machining to restore the chromium oxide film. Select Passivate on the quote finish list; it adds finish days on the production clock.
Passivation is a chemical clean and oxide restore. Zinc plate and nickel plate are separate finishes with their own pages, and you can select them on the quote. No plating-line count is claimed.
| Item | Spec |
|---|---|
| Dade a wɔde gyina so | Nneɛma a ɛnyɛ den (304 / 316) . |
| DFM afotu | Ɛnyɛ nea wɔde besi plating ananmu |
No — passivation is a chemical clean/oxide restore, not a plated coating.
AI Instant Reference Quote + engineering review within 12 business hours.
Adwuma email a wɔpɛ ([email protected]). Ankorankoro nkrataa a wɔde mena no yɛ OK. Optional — download no da so ara yɛ adwuma.