Zoryra Precision

CNC Materials & Surface Finish Atlas

Select grades and finishes in the quote form — engineering review for special alloys. Match finish to material (e.g. anodize for aluminum).

pedasu dentu AI gosi-gosi prisu

Es paj e pa un orsamentu CNC. Fala kusa, sima alumíniu 6061 ô asu ki ka oxida, poi toleránsia na dezeñu, i kantidadi. Tenpu di sempri e 8–10 dia, di un pédsu.

abri prisu forsa-makina
faze-pedasu stóf-s

skoyi-un gradus kel-la sirvi bu projeitu

Es paj e pa un orsamentu CNC. Fala kusa, sima alumíniu 6061 ô asu ki ka oxida, poi toleránsia na dezeñu, i kantidadi. Tenpu di sempri e 8–10 dia, di un pédsu.

Es paj e pa un orsamentu CNC. Fala kusa, sima alumíniu 6061 ô asu ki ka oxida, poi toleránsia na dezeñu, i kantidadi. Tenpu di sempri e 8–10 dia, di un pédsu.

pedasu pa-meiu pedasu
Showing 25 grades

alumíniu6

alumíniu 6061

alumíniu 6061

CNC korta-makinapesalijeiru-lijeiru purmeru-faze

AKA: Al6061-T6 / EN-AW6061

txavi pedasu
WorkhorseWeldableCost-effective

Es paj e pa un orsamentu CNC. Fala kusa, sima alumíniu 6061 ô asu ki ka oxida, poi toleránsia na dezeñu, i kantidadi. Tenpu di sempri e 8–10 dia, di un pédsu.

Aluminum 6082

Aluminum 6082

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: Al6082 / EN-AW6082

txavi pedasu
Medium strengthThermal conductivityWeldable

Medium strength with good weldability/thermal conductivity for structures.

Aluminum 5052

Aluminum 5052

CNC korta-makinapesa

AKA: Al5052 / sheet-metal favorite

txavi pedasu
Corrosion resistantBend-friendlyHousings

Corrosion-resistant; common for sheet bend housings and light CNC.

Aluminum 5083

Aluminum 5083

CNC korta-makinapesa

AKA: Al5083 / marine-grade corrosion resistance

txavi pedasu
High corrosion resistanceModerate strengthPlate stock

Moderate strength, high corrosion resistance for plates/structures.

alumíniu 7075

alumíniu 7075

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: Al7075-T6 / EN-AW7075

txavi pedasu
High strengthFatigue resistantMachines well

Es paj e pa un orsamentu CNC. Fala kusa, sima alumíniu 6061 ô asu ki ka oxida, poi toleránsia na dezeñu, i kantidadi. Tenpu di sempri e 8–10 dia, di un pédsu.

Aluminum 2024

Aluminum 2024

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: Al2024 / aerospace-class strength

txavi pedasu
High strengthFatigue performanceLimited weldability

High-strength aerospace-class Al; welding limited — confirm temper on drawing.

asu-ka-feruja4

asu-ka-feruja 304

asu-ka-feruja 304

CNC korta-makinapesalijeiru-lijeiru purmeru-faze

AKA: SS304 / 1.4301

txavi pedasu
General stainlessPassivate OKNo anodize

tudu-kusa-razoin asu-ka-feruja; pasiva/brilya — ka kapa-oksidu.

asu-ka-feruja 316

asu-ka-feruja 316

CNC korta-makinapesalijeiru-lijeiru purmeru-faze

AKA: SS316 / better corrosion resistance

txavi pedasu
Better corrosion resistanceMedical/lab commonPassivate OK

Es paj e pa un orsamentu CNC. Fala kusa, sima alumíniu 6061 ô asu ki ka oxida, poi toleránsia na dezeñu, i kantidadi. Tenpu di sempri e 8–10 dia, di un pédsu.

Stainless 303

Stainless 303

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: SS303 / free-machining

txavi pedasu
Free-machiningVolume small partsTurn/mill friendly

Free-machining stainless for turned/milled volume small parts.

17-4PH stainless

17-4PH stainless

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: 17-4PH / 1.4542

txavi pedasu
Precipitation hardeningHigh strengthCall out temper

Precipitation-hardening stainless; call out heat-treat condition on drawings.

asu4

Mild steel

Mild steel

CNC korta-makinapesalijeiru-lijeiru purmeru-faze

AKA: A36 / Q235 class

txavi pedasu
EconomicalPowder / black oxideEasy to machine

Economical structural steel; powder / black oxide / zinc common.

1045 karbonu asu

1045 karbonu asu

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: 1045 / C45

txavi pedasu
Medium carbonShaftsHeat-treatable

Medium-carbon steel; stronger than mild steel — common for shafts.

4140 mistura-asu asu

4140 mistura-asu asu

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: 4140 / 42CrMo class

txavi pedasu
High strengthTough / impactConfirm heat treat

Alloy structural steel; confirm heat treatment with engineering.

xavi asu (tudu-kusa)

xavi asu (tudu-kusa)

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: general tool-steel class

txavi pedasu
Wear resistantTooling classSpecify grade in notes

Wear/tooling class — specify exact grade in notes (SKD / S136 etc. via engineer).

titaniu1

titaniu-poku-6alumíniu-4V titaniu

titaniu-poku-6alumíniu-4V titaniu

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: TC4 / Grade 5

txavi pedasu
High strength-to-weightLightweightSlower machining

High strength-to-weight; slower machining — engineer review for complex parts.

kobre mistura-asu-s3

kobre-amarelu

kobre-amarelu

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: Brass / free-cutting copper alloy

txavi pedasu
Free-cuttingConductiveFittings / cosmetics

Free-cutting; good conductivity — fittings and cosmetic parts.

kobre-maron

kobre-maron

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: Bronze

txavi pedasu
Wear resistantBushingsNote exact grade

Common for wear bushings — note exact grade when required.

kobre C110

kobre C110

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: C110 / ETP copper

txavi pedasu
High conductivityThermalElectrical / heat sinks

High conductivity for thermal/electrical parts.

ofisi-tekniku plastikus7

ABS

ABS

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: ABS engineering plastic

txavi pedasu
General housingsEasy machiningFixtures

General housings/fixtures; easy to machine.

Nylon (poliamida)

Nylon (poliamida)

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: PA / Nylon

txavi pedasu
ToughGears / slidersMoisture swell

Tough for gears/sliders — watch moisture swell on fits.

POM / Acetal

POM / Acetal

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: POM / Delrin-class

txavi pedasu
Dimensionally stableWear resistantPrecision plastics

Dimensionally stable and wear-resistant for precision plastic parts.

polikarbonatu (pedasu-un)

polikarbonatu (pedasu-un)

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: PC

txavi pedasu
Clear optionsImpact toughnessStress-crack care

Clear/translucent housings possible — watch stress cracking.

akriliku / PMMA

akriliku / PMMA

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: PMMA / acrylic

txavi pedasu
Optical / displayPolishableWatch brittleness

Optical/display parts; edges can be polished.

PTFE / Teflon

PTFE / Teflon

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: PTFE

txavi pedasu
Chemically inertLow frictionLow stiffness

Chemically inert, low friction — low stiffness needs design care.

PEEK

PEEK

CNC korta-makinalijeiru-lijeiru purmeru-faze

AKA: PEEK high-performance plastic

txavi pedasu
High tempHigh strengthPremium cost

High-temp/high-strength plastic; premium — for demanding duty.

akabu-fas pedasu

modi-korta · stóf-s · tenpu-spera-ora pedasu

Es paj e pa un orsamentu CNC. Fala kusa, sima alumíniu 6061 ô asu ki ka oxida, poi toleránsia na dezeñu, i kantidadi. Tenpu di sempri e 8–10 dia, di un pédsu. Prisu AI e guia. Kunpra un pédsu antis di un monti grandi.

trabadju
trabadju
  • stóf-salumíniu / asu / asu-ka-feruja / plastikus
  • tenpu-spera pedasupedasu +0 dia (pedasu pedasu)
  • skrevi-pokuxavi pedasu pedasu; pedasu pá pedasu & sirvi-junta fasis.
konta
konta
  • stóf-spedasu alumíniu / asu-ka-feruja
  • tenpu-spera pedasu~+1–2 dia (pedasu pedasu)
  • skrevi-pokupedasu pedasu; pedasu antis kapa-oksidu.
kapa-oksidu (klaru / pretu / duru)
kapa-oksidu (klaru / pretu / duru)
  • stóf-salumíniu pedasu
  • tenpu-spera pedasu~+2–4 dia; akabamentu pedasu
  • skrevi-pokuxama fora pedasu riba pedasu; ka pá asu-ka-feruja.
pasivason
pasivason
  • stóf-sSS304 / SS316
  • tenpu-spera pedasu~+1–3 dia
  • skrevi-pokupedasu feruja rezistensia; pedasu ku brilya.
pu-kapa
pu-kapa
  • stóf-sasu / alumíniu struturas
  • tenpu-spera pedasu~+3–5 dia
  • skrevi-pokupedasu filmi; pedasu roskas & pedasu.
brilya / pedasu
brilya / pedasu
  • stóf-sasu-ka-feruja / alumíniu
  • tenpu-spera pedasu~+1–3 dia (pedasu gradu)
  • skrevi-pokumanda purmeru-pesa du Ra pedasu pá pedasu.

Metals

Al6061/7075/5052, SS304/316/303, mild steel, 4140, brass, copper. Titanium on request via engineering review.

Plastics

ABS, Nylon, POM, PC, PEEK and similar engineering plastics common in fixtures and housings.

Finishes

As-machined, bead blast, clear/black/hard anodize, powder coat, passivate, polish, brushed, chromate, zinc plate, black oxide. Plating beyond the list is discussed case by case.

Lead-time impact (production clock)

Reference: blast +1–2d, anodize +2–4d, powder +3–5d. Courier days stay separate on the quote. See the problem guide on masking before you freeze PO dates.

Compatibility tips

Anodize is typical for aluminum; passivation for stainless; black oxide / zinc for steels. Cosmetic anodize needs masking notes on drawings — thermal faces on electronics often stay as-machined.

Certificates

Material certificates / heat-lot traceability available per order agreement when selected — no invented cert numbers on marketing pages.

Capability specs & DFM

ItemSpec
pedasuPesa dron: motora, brasu, liso, bandexa bataria. Alumíniu 6061. 8–10 dia. Es paj e pa un orsamentu CNC. Fala kusa, sima alumíniu 6061 ô asu ki ka oxida, poi toleránsia na dezeñu, i kantidadi. Tenpu di sempri e 8–10 dia, di un pédsu.
plastikusPOM, Nylon, pedasu-un, PTFE (pedasu pedasu)
akabu-fasistrabadju, kapa-oksidu, konta, pasiva, pu-kapa
pedasustóf pedasu ten-li pa-un enkomenda pedasu
DFM pedasuEs paj e pa un orsamentu CNC. Fala kusa, sima alumíniu 6061 ô asu ki ka oxida, poi toleránsia na dezeñu, i kantidadi. Tenpu di sempri e 8–10 dia, di un pédsu.

FAQ

Can I anodize stainless?

Anodize is typical for aluminum. For stainless, passivation or polish is the usual path — confirm in RFQ.

Is hard anodize available?

Yes — selectable as Hard anodize in the quote finish list for aluminum parts.

How many days does finishing add?

Reference: blast +1–2d, anodize +2–4d, powder +3–5d — see the finish atlas. Final days are itemized on the quote.

Where do I configure finish for a real part?

On the quote page — pick material + finish there, then engineering confirms masking / thermal keep-outs.

Next: upload CAD or talk to an Engineer

AI Instant Reference Quote + engineering review within 12 business hours.

AIprisukarta-netu
PDF

Es paj e pa un orsamentu CNC. Fala kusa, sima alumíniu 6061 ô asu ki ka oxida, poi toleránsia na dezeñu, i kantidadi. Tenpu di sempri e 8–10 dia, di un pédsu.

Es paj e pa un orsamentu CNC. Fala kusa, sima alumíniu 6061 ô asu ki ka oxida, poi toleránsia na dezeñu, i kantidadi. Tenpu di sempri e 8–10 dia, di un pédsu.

CNC Materials & Finishes Atlas | Anodize Blast Passivate Powder