Restore corrosion resistance after machining stainless — typical for SS304 / SS316 export jobs.

Material match

Passivation is intended for stainless families. Aluminum should use anodize instead.

When buyers ask for it

SS304 / SS316 export jobs often add passivation after machining to restore the chromium oxide film. Select Passivate on the quote finish list; it adds finish days on the production clock.

Not a plated coating

Passivation is a chemical clean and oxide restore. Zinc plate and nickel plate are separate finishes with their own pages, and you can select them on the quote. No plating-line count is claimed.

Capability specs & DFM

ItemSpec
Base metalHindi kinakalawang (304 / 316)
Tip sa DFMHindi isang kapalit para sa kalupkop

FAQ

Is passivation the same as electroplating?

No — passivation is a chemical clean/oxide restore, not a plated coating.

Next: upload CAD or talk to an Engineer

AI Instant Reference Quote + engineering review within 12 business hours.

AIQuoteEmail
PDF

Mas gusto ang email sa trabaho ([email protected]). Ang personal na mail ay OK. Opsyonal — gumagana pa rin ang pag-download.

Gagamitin lang namin ang email sa trabahong ito para ipadala ang item na ito at para sagutin ang iyong mga tanong sa engineering (quote, lead time, mga drawing).

Stainless Passivation | Zoryra Precision CNC