Problem: AI Cold Plate Flatness Fails After Finish — Keep the Thermal Face Clean

Problem: accelerator cold plates meet thickness in-process, then after anodize or plating the contact face bows past 0.05–0.1 mm and TIM / liquid interface leaks heat.

Root cause: whole-part cosmetic finish with no masking; copper chosen late without lead-time buffer; sealing ports underspecified on the PDF.

Fix: as-machined thermal face; mask threads / ports; lock Al vs Cu on the first quote; sample flatness before ship.

Lead sketch: Standard ≈ 8–10 days with finish; Express when blank + light finish allow. Courier days stay separate.

Next: open the AI hardware industry page, then upload STEP + PDF on the quote page with flatness callouts.

AIQuoteEmail
PDF

ናይ ስራሕ ኢመይል ተመራጺ ([email protected]) ። ናይ ውልቀ-ሰብ ደብዳበ ጽቡቕ እዩ ። ኣማራጺ — እቲ ምውራድ ገና ይሰርሕ ።

ነዚ ኢመይል ስራሕ እዚ ንምልኣኽን ንናይ ምህንድስና ሕቶታትካ ንምምላስን ጥራይ ኢና እንጥቀመሉ (ጥቕሲ ፡ ግዜ መሪሕነት ፡ ስእሊ) ።

Problem: AI Cold Plate Flatness Fails After Finish — Keep the Thermal Face Clean — Zoryra Precision