Problem: AI Cold Plate Flatness Fails After Finish — Keep the Thermal Face Clean

Problem: accelerator cold plates meet thickness in-process, then after anodize or plating the contact face bows past 0.05–0.1 mm and TIM / liquid interface leaks heat.

Root cause: whole-part cosmetic finish with no masking; copper chosen late without lead-time buffer; sealing ports underspecified on the PDF.

Fix: as-machined thermal face; mask threads / ports; lock Al vs Cu on the first quote; sample flatness before ship.

Lead sketch: Standard ≈ 8–10 days with finish; Express when blank + light finish allow. Courier days stay separate.

Next: open the AI hardware industry page, then upload STEP + PDF on the quote page with flatness callouts.

AIQuoteEmail
PDF

Email serbisu nian prefere liu ([email protected]). Korreiu pesoál di'ak. Opsionál — download funsiona nafatin.

Ami sei uza email serbisu ida-ne'e de'it atu haruka sasán ida-ne'e no atu hatán ba ita-boot nia pergunta sira kona-ba enjeñaria (sitasaun, tempu, dezeñu sira).

Problem: AI Cold Plate Flatness Fails After Finish — Keep the Thermal Face Clean — Zoryra Precision