Standard i zakonshëm ~10 ditë (prod + skicë me ajër) · Ekspres ~6 ditë · vizatim / DFM

2026-08-10 · 4 min

Problem: AI Cold Plate Flatness Fails After Finish — Keep the Thermal Face Clean

Problem: accelerator cold plates meet thickness in-process, then after anodize or plating the contact face bows past 0.05–0.1 mm and TIM / liquid interface leaks heat.

Root cause: whole-part cosmetic finish with no masking; copper chosen late without lead-time buffer; sealing ports underspecified on the PDF.

Fix: as-machined thermal face; mask threads / ports; lock Al vs Cu on the first quote; sample flatness before ship.

Lead sketch: Standard ≈ 8–10 days with finish; Express when blank + light finish allow. Courier days stay separate.

Next: open the AI hardware industry page, then upload STEP + PDF on the quote page with flatness callouts.

KuotëAIEmail
PDF

Preferohet email-i i punës ([email protected]). Email-i personal është OK. Opsionale — shkarkimi vazhdon të funksionojë.

Ne do të përdorim këtë email pune vetëm për të dërguar këtë artikull dhe për t’iu përgjigjur pyetjeve tuaja inxhinierike (ofertë, kohëzgjatje, vizatime).

Problem: AI Cold Plate Flatness Fails After Finish — Keep the Thermal Face Clean — Zoryra Precision