Fenitra mahazatra ~10 andro (prod + air sketch) · Haingam-pamokarana ~6 andro · sary / DFM

2026-08-10 · 4 min

Problem: AI Cold Plate Flatness Fails After Finish — Keep the Thermal Face Clean

Problem: accelerator cold plates meet thickness in-process, then after anodize or plating the contact face bows past 0.05–0.1 mm and TIM / liquid interface leaks heat.

Root cause: whole-part cosmetic finish with no masking; copper chosen late without lead-time buffer; sealing ports underspecified on the PDF.

Fix: as-machined thermal face; mask threads / ports; lock Al vs Cu on the first quote; sample flatness before ship.

Lead sketch: Standard ≈ 8–10 days with finish; Express when blank + light finish allow. Courier days stay separate.

Next: open the AI hardware industry page, then upload STEP + PDF on the quote page with flatness callouts.

Tenynalainatamin'nyAIEmail
PDF

Aleony mailaka momba ny asa ([email protected]). OK ihany koa ny mailaka manokana. Safidy — mbola miasa ihany ny fisintomana.

Hampiasa ity mailaka momba ny asa ity fotsiny izahay mba handefasana ity zavatra ity sy hamaliana ny fanontaniana momba ny injeniera (vidiny, fotoana mitarika, sarin-drafitra).

Problem: AI Cold Plate Flatness Fails After Finish — Keep the Thermal Face Clean — Zoryra Precision